3M 5200 ?? - Bubman1 - 04-15-2024

Do any of you have experience with this marine grade silicon it says it can take up to 5 days to cure and I'm on day four and it's sill tacky. Thanks


RE: 3M 5200 ?? - Kent - 04-15-2024

I have used it and it does take a long time to cure. It would also depend on temperature and humidity. I would give it another day or two.


RE: 3M 5200 ?? - gmwahl - 04-16-2024

Keep it above 70 degrees and give it at least a week. Works great, but it is a pain to wait for it to cure.

Mike


RE: 3M 5200 ?? - Bubman1 - 04-16-2024

It started setting up yesterday I'm hoping it's ready by this weekend I got an itch for something to pull on my line thanks guys


RE: 3M 5200 ?? - BearLakeFishGuy - 04-17-2024

Pretty sure they sell a "fast cure" 5200 in addition to the regular one. At least they used to. I think it was 24 hr.